salem steel 316 plates are a piece of the austenitic group of treated steel and is the most broadly utilized assortments of impeccable plate. 316 evaluations contain a more significant level of Nickel than 304 giving it an improved erosion obstruction more than 304 evaluations. 316 plate is a decent alternative for marine applications because of a decent environmental consumption opposition. 316 is a low carbon change to 316 evaluation. It is basic practice for 316 to be double affirmed as 316 and 316. The low carbon science of 316 joined with an expansion of nitrogen empowers 316 to meet the mechanical properties of 316.
specification | ASTM A240 / ASME SA240 |
Grade | ASTM A240 Grade 316 |
Type | ASTM A240 Type 316 Plate |
Standard | ASTM, AISI, SUS, JIS, EN, DIN, GB, ASME, etc |
Technique | Cold/Hot Rolled 316 Stainless Steel plate |
Size | 6000mm x 2000mm / 4000mm x 2000mm / 4000mm x 1500mm / 3000mm x 1500mm / 2500mm x 1250mm / 2000mm x 1000mm. * Please contact us for non-standard sizes and lengths |
Hardness | Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc. |
Form | SS 316 Foils, Rolls, Plain Sheet, Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Blank (Circle), Ring (Flange) |
STANDARD | UNS | WERKSTOFF NR. | EN | AFNOR | BS | GOST | JIS |
SS 316 | S31600 | 1.4401 / 1.4436 | X5CrNiMo17-12-2 / X3CrNiMo17-13-3 | Z7CND17‐11‐02 | 316S31 / 316S33 | - | SUS 316 |
SS 316L | S31603 | 1.4404 / 1.4435 | X2CrNiMo17-12-2 / X2CrNiMo18-14-3 | Z3CND17‐11‐02 / Z3CND18‐14‐03 | 316S11 / 316S13 | 03Ch17N14M3 / 03Ch17N14M2 | SUS |
Grade
|
C
|
Mn
|
Si
|
P
|
S
|
Cr
|
Mo
|
Ni
|
N
|
|
316
|
Min
|
-
|
-
|
-
|
0
|
-
|
16.0
|
2.00
|
10.0
|
-
|
Max
|
0.08
|
2.0
|
0.75
|
0.045
|
0.03
|
18.0
|
3.00
|
14.0
|
0.10
|
|
316L
|
Min
|
-
|
-
|
-
|
-
|
-
|
16.0
|
2.00
|
10.0
|
-
|
Max
|
0.03
|
2.0
|
0.75 |
0.045
|
0.03
|
18.0
|
3.00
|
14.0
|
0.10
|
|
316H
|
Min
|
0.04
|
0.04
|
0
|
-
|
-
|
16.0
|
2.00
|
10.0
|
-
|
Max
|
0.10
|
0.10
|
0.75
|
0.045
|
0.03
|
18.0
|
3.00
|
14.0
|
-
|
Grade
|
Tensile Str
(MPa) min |
Yield Str
0.2% Proof (MPa) min |
Elong
(% in 50mm) min |
Hardness
|
|
Rockwell B (HR B) max
|
Brinell (HB) max
|
||||
316
|
515
|
205
|
40
|
95
|
217
|
316L
|
485
|
170
|
40
|
95
|
217
|
316H
|
515
|
205
|
40
|
95
|
217
|