Salem stainless steel are had practical experience in the creation of Stainless Steel 202 Rods. We are a main assembling firm offering these bars in different principles, particulars and custom measurements. We likewise give treated steel poles resistance limit and machining remittances for use in different applications. We are sourced with programmed machines and gear that makes us ready to create items that meet the necessities of client applications. We oversee separate planning division and most recent generation where we draw items according to the national and global measures of value. Under explicit mechanical codes, items are produced utilizing great nature of materials. Stainless Steel 202 Rods are chromium and manganese hardened steel from austenitic family. In any case, it has a moderate measure of nitrogen, copper and nickel content. These bars are adjusted with alloying components. In the wake of toughening activity, it gets an austenitic structure. The arrangement of nitrogen content offer raised quality and raise formability. These bars are perfect to use in basic applications. Because of the copper content its work solidifying rates is less.
Specifications | ASTM A276, A479 / ASME SA276, SA479 |
Standard | BS, JIS, ASTM, ASME, EN, AISI, DIN, |
Size Range | 3.17 MM TO 350 MM DIA |
Diameter | 25mm to 152mm |
Finish | Bright, Polish, Bright, Rough Turned, Grinding, Centreless Ground & Black |
Tolerance | h8, h9(DIN 671), h10, h11, ASTM A484, DIN 1013 |
Condition | Cold Drawn, Polished Cold Drawn Centreless Ground & Polished, Annealed round bar |
Technique | Stainless Steel 316 Hot Rolled, Cold Rolled, Cold Drawn, Forged Round Bar, Rod |
Form | Round, Rod, Precision Ground Bar, Square, Round Rod, Hollow, Hex (A/F), Triangle, Rectangle, Threaded, T-Bar, Half Round Bar, Flat Bar, Rings, Blocks, Billet, Ingot, I/H Bar, Angle Bar, Channel Bar, Profiles, Forging Etc. |
Element |
Content (%) |
---|---|
Iron, Fe |
68 |
Chromium, Cr |
17- 19 |
Manganese, Mn |
7.50-10 |
Nickel, Ni |
4-6 |
Silicon, Si |
≤ 1 |
Nitrogen, N |
≤ 0.25 |
Carbon, C |
≤ 0.15 |
Phosphorous, P |
≤ 0.060 |
Sulfur, S |
≤ 0.030 |
Properties |
Metric |
Imperial |
---|---|---|
Tensile strength |
515 MPa |
74694 psi |
Yield strength |
275 MPa |
39900 psi |
Elastic modulus |
207 GPa |
30000 ksi |
Poisson's ratio |
0.27-0.30 |
0.27-0.30 |
Elongation at break |
40% |
40% |
Physical Property |
Value |
---|---|
Density |
7.80 g/cm³ |
Thermal Expansion |
17 x10^-6 /K |
Modulus of Elasticity |
200 GPa |
Thermal Conductivity |
15 W/m.K |